The Infona portal uses cookies, i.e. strings of text saved by a browser on the user's device. The portal can access those files and use them to remember the user's data, such as their chosen settings (screen view, interface language, etc.), or their login data. By using the Infona portal the user accepts automatic saving and using this information for portal operation purposes. More information on the subject can be found in the Privacy Policy and Terms of Service. By closing this window the user confirms that they have read the information on cookie usage, and they accept the privacy policy and the way cookies are used by the portal. You can change the cookie settings in your browser.
Chitosan derivatives were obtained by chemical (MW of 6 kDa, DD 99% - Ch6/99; MW13 kDa, DD 98% - Ch13/98) and enzymatic (MW of 5 kDa, DD 85% - Ch5/85; MW of 10 kDa, DD 85% - Ch10/85) depolymeri-sation of chitosan with a MW of 334 and 1000 kDa. Chitosan derivatives (almost identical MW pairs and different DD) possessed insignificant an-ticoagulant activity, did not promote human platelet aggregation...
The article presents the effectiveness of orthophosphate sorption from aqueous solutions depending on the deacetylation degree of chitosan flakes. The first stage of the research was to determine the pH value at which the sorption process was the most effective (from the pH range 2–11). In the second stage, research was carried out to determine the maximum sorption capacities of chitosan with deacetylation...
The influence of the degree of deacetylation of chitosan from the range of DD = 75–90% on the effectiveness of sorption of nitrates from aqueous solutions was investigated. The scope of the research included: determining the effect of pH on the effectiveness of N-NO3 binding on chitosan sorbents and determining the sorption capacity of chitosan sorbents with different degrees of deacetylation after...
In the paper sorption capacity of chitosan having a deacetylation degree DD=75%, DD=85% and DD=90% relatively to the Reactive Black 5 were compared. Studies on the effectiveness of the dye sorption were carried out in a wide pH range – from 3 to 11. For each of the tested chitosan sorbents, sorption capacity has been determined. The results were described by isotherms Freundlich and Lagmuir isotherms,...